Nitronic 40





Detay
LORK GROUP-wo kalite NITRONIC 40 se yon gwo-Manganese asye pur ak gwo fòs ak ekselan rezistans nan korozyon nan tanperati ki wo.
Pwodwi Deskripsyon
LORK GROUP-wo kalite NITRONIC 40 se yon gwo-Manganese asye pur ak gwo fòs ak ekselan rezistans nan korozyon nan tanperati ki wo. Nitronic 40 ka fabrike ak fasilman soudab.
Nitronic 40 te itilize pou pwosesis chimik, ekipman kontwòl polisyon ak divès kalite konpozan motè avyon.
Fòm pwodwi
AMS 5656 Bar / Fil
AMS 5595 Fèy / Plak / Strip
AMS 5561 Tib soude
AMS 5562 Tib san pwoblèm
AMS 5656 bag / extrusions
Mil-t-9821
ASTM A276 / ASME SA276
ASTM A412 / ASME SA412
ASTM A580 / ASME SA580
UNS S21906
Nitronic 40 konpozisyon chimik
|
Eleman |
Kontni (%) |
|
C |
0.04 Max |
|
P |
0.060 Max |
|
Si |
1.00 Max |
|
NI |
5.5-7.5 |
|
Fe |
Bal |
|
Mn |
8-10 |
|
S |
0.030 Max |
|
Cr |
19-21.5 |
|
N |
0.15-0.40 |
|
Mwa |
0.75 max |
|
CU |
0.75 max |
Nitronic 40 pwopriyete mekanik (Minium)
|
Ultim fòs rupture |
655 MPa |
|
Sede fòs |
330 MPa |
|
Elongasyon 50mm % |
35 |
|
Brinell dite |
241 |
Nitronic 40 Aplikasyon
- Adezif ak soufle
- Eleman motè avyon
- Sèvis kriyojenik
- Pwosesis chimik