MP35N Cobalt alyaj (ASTM F-562, ISO 5832-6)

MP35N Cobalt alyaj (ASTM F-562, ISO 5832-6)

MP35N se yon alyaj cobalt-nikèl-chromium-molybdène ki fèt espesyalman pou enplantasyon chirijikal, ki konfòme yo ak estanda ASTM F562 ak ISO 5832-6. Li se materyèl chwa pou aparèy implantable alontèm tankou fil pacemaker ak fil gid.
Voye rechèch

MP35N Cobalt alyaj (ASTM F-562, ISO 5832-6)

 

MP35N (UNS R30035, ASTM F562, ISO 5832-6) se yon nikèl-cobalt-alyaj austenitic ki gen yon kontni cobalt apeprè 35%. Dapre estanda ASTM F562 ak ISO 5832-6, MP35N deziyen klèman kòm yon alyaj kobalt-nikèl-kwòm-molibdèn pou enplantasyon chirijikal; li espesyalman enjenyè pou enplantasyon imen alontèm, satisfè kondisyon solid pou biocompatibility, pite, ak rezistans fatig.

 

Sètifika materyèl founisè anjeneral lis ASTM F562, ISO 5832-6, ak BS 7252-6 kòt-kòt kòm prèv prensipal kalifikasyon medikal-klas materyèl la.

 

Pou aparèy implantable, sa vle di sa ki annapre yo:

Fatig krak inisyasyon: Patikil difisil yo aji kòm pwen konsantrasyon estrès, deklanche fant anba chay pulsatile alontèm -e ki kapab mennen nan echèk twò bonè nan aparèy tankou kondwi pesmekè.

Pwosesis domaj: Pandan desen frèt, patikil sa yo ka grate mouri a, sa ki lakòz domaj sifas sou fil la ki plis konpwomi pèfòmans fatig.

 

An konsekans, se vreman wo -fyabilite medikal- MP35N klas medikal ki pwodui ak nivo Titàn ak nitwojèn kenbe byen anba limit maksimòm ki espesifye nan estanda yo. Patant yo endike klèman ke pwodwi siperyè medikal -ka kenbe nivo Titàn pi ba pase 0.01%-oswa menm ba ke 0.001%-konsa anpeche fòmasyon enklizyon danjere nan sous la.

 

Dimansyon ak pwofil ki kouvri pa Estanda debaz la

 

Ba-Pwodwi ki gen fòm wonn, rektangilè, oswa lòt fòm konplèks, livrezon dwat epi koupe nan longè espesifik.
Fil amann-Pwodwi ki gen fòm wonn, rektangilè, oswa lòt fòm konplèks ki gen yon koup transvèsal inifòm sou tout longè yo, ak yon dyamèt oswa epesè mwens pase 1.60 mm [0.063 pous], yo bay nan bobin, sou bobin, oswa nan lòt fòm anbalaj jan sa espesifye.
Fil-Pwodwi ki gen fòm wonn, rektangilè, oswa lòt fòm konplèks ki gen yon koup transvèsal inifòm sou tout longè yo, ak yon dyamèt oswa epesè mwens pase 4.76 mm [0.1875 pous], yo bay nan bobin, sou bobin, oswa nan lòt fòm anbalaj jan sa espesifye.

 

konpozisyon chimik

ASTM F-562

 

Eleman
min
max
C -- 0.025
Mn -- 0.15
Si -- 0.15
P -- 0.015
S -- 0.010
Kr 19.0 21.0
Ni 33.0 37.0
Mo 9.0 10.5
Fe -- 1.0
Ti -- 1.0
B -- 0.015
Co Balans  

 

Pwopriyete mekanik (pwodwi ba)

 

Kondisyon
Fòs rupture
MPa [psi]
Fòs Sede (0.2% Offset)
MPa [psi]
Elongasyon
min, %
Rediksyon nan zòn
min, %
Solisyon-rekwit
793 jiska 1069 [115 000 rive 155 000]
241 jiska 586 [35 000 rive 85 000]
50.0 65.0
Fwad-te travay
mwayen difisil
1000 [145 000] min.
655 [95 000] min.
20.0 60.0
difisil
1207 [175 000] min.
1000 [145 000] min.
10.0 50.0
Fwad-travay ak aje
1793 [260 000] min.
1586 [230 000] min. 8.0 35.0

 

Pwopriyete mekanik-Pwodwi Fil (d Pi gran pase oswa egal a 1.6 mm [0.063 pous.])

 

Kondisyon
Fòs rupture
MPa [psi]
Fòs Sede (0.2% Offset)
MPa [psi]
Elongasyon
min, %
Rediksyon nan zòn
min, %
Solisyon-rekwit
793 jiska 1069 [115 000 rive 155 000]
241 jiska 586 [35 000 rive 85 000]
50.0 65.0
Fwad-te travay
mwayen difisil
1000 [145 000] min.
655 [95 000] min.
20.0 60.0
difisil
1207 [175 000] min.
1000 [145 000] min.
10.0 50.0
Fwad-travay ak aje
1793 [260 000] min.
1586 [230 000] min.
8.0 35.0

 

Pwopriyete mekanik -Fil amann (d < 1.6 mm [0.063 pous.])

 

Dyamèt, mm [pous]
Rkwit
Fòs rupture,
MPapsi]
Elongasyon
min, %
<1.600 to 1.473
[<0.063 to 0.058]
827 jiska 1034
[120 000 rive 150 000]
40.0
<1.473 to 0.864
[<0.058 to 0.034]
862 rive 1069
[125 000 rive 155 000]
40.0
<0.864 to 0.406
[<0.034 to 0.016]
931 jiska 1138
[135 000 rive 165 000]
40.0
<0.406 to 0.0762
[<0.016 to 0.003]
1000 jiska 1207
[145 000 rive 175 000]
30.0
<0.0762 to 0.0508
[<0.003 to 0.002]
1034 jiska 1310
[150 000 rive 190 000]
30.0
<0.0508
[<0.002]
1172 jiska 1448
[170 000 rive 210 000]
25.0

 

Dyamèt, mm [pous]
Fwad-Travay
 
 
Difisil
Prentan
 
Fòs rupture,
MPa [psi]
Elongasyon
min, %
Fòs rupture,
MPa [psi]
Elongasyon
min, %
<1.600 to 1.473
[<0.063 to 0.058]
1655 rive 1862
[240 000 rive 270 000]
2.0
1862 rive 2068
[270 000 rive 300 000]
2.0
<1.473 to 0.864
[<0.058 to 0.034]
1689 jiska 1896
[245 000 rive 275 000]
2.0
1896 jiska 2103
[275 000 rive 305 000]
2.0
<0.864 to 0.406
[<0.034 to 0.016]
1758 rive 1965
[255 000 rive 285 000]
2.0
1965 rive 2172
[285 000 rive 315 000]
2.0
<0.406 to 0.0762
[<0.016 to 0.003]
1827 jiska 2034
[265 000 rive 295 000]
2.0
2034 jiska 2241
[295 000 rive 325 000]
2.0
<0.0762 to 0.0508
[<0.003 to 0.002]
1896 jiska 2103
[275 000 rive 305 000
2.0
2103 rive 2310
[305 000 rive 335 000]
2.0
<0.0508
[<0.002]
1999 jiska 2275
[290 000 rive 330 000]
1.8
2206 jiska 2482
[320 000 rive 360 000]
1.8

 

Pwen pwosesis kle yo

 

Machining MP35N (konfòme ak ASTM F562 / ISO 5832-6 estanda) se yon defi paske li yo trè rapid travay -difisi pousantaj- twa a senk fwa nan asye pur 316L -fè li yon difisil-alyaj machin. Estrateji D' dwe pwepare pou kondisyon materyèl la nan moman traitement.

 

Machining nan Solisyon-Eta Trete (Rekuit).
Pandan ke MP35N reyalize pi gwo fòs li yo atravè yon konbinezon de travay frèt ak aje, materyèl la vin trè difisil nan kondisyon ki gen laj (rive 45-55 HRC). Machin konvansyonèl se nòmalman enposib nan etap sa a, kite fanm k'ap pile oswa Machining Discharge Elektrik (EDM) kòm sèlman opsyon ki solid.

 

Flux travay rekòmande a se: Pwokire stock ba oswa vid tib nan solisyon an-trete (rekwit) eta (dite apeprè. 25–32 HRC) → Fini tout operasyon degrosaj ak semi-fini → Fè tretman final la aje pou reyalize fòs ki nesesè yo. Akizisyon pre-stock ki gen laj yo ta dwe konsidere sèlman si pati a mande pou ekstrèm presizyon epi li pa ka tolere deformation pandan aje; nan ka sa yo, alokasyon machin ak paramèt pwosesis yo dwe planifye separeman.

 

Koupe Paramèt (Referans pou vire nan solisyon an-Eta trete)
Lè w ap koupe nan eta trete solisyon an-, yon apwòch "ba vitès, gwo manje, ak koupe gwo twou san fon" esansyèl pou anpeche zouti nan fwote kont travay la-kouch ki fè tèt di toujou olye pou yo koupe l:

Seleksyon Zouti: Yo dwe itilize zouti Carbide (K-klas oswa PVD-kouvwi); itilizasyon gwo-sye vitès (HSS) entèdi entèdi.

Machining in the Solution-Treated (Annealed) State

 

Konfime fòm pwodwi ak estati

 

Anvan nou bay yon sitasyon, nou pral diskite sou espesifikasyon teknik sa yo avèk ou:

 

  • Fòm: ba wonn, ba plat, fil, oswa fòje?
  • Dimansyon: Dyamèt / Longè Side, Longè
  • Kondisyon: Rekwit (mou) oswa Fwad-travay/Aje (difisil)?
  • Fini sifas: vire, tè, marinated, oswa poli?
  • Kondisyon pou tretman chalè: Èske founisè a oblije fè tretman frèt ak aje anvan chajman?

 

 